30 vol. perxoide

R

renegade_cowboy

Guest
I use 40 volume straight and gay on various stains. You might also want to try some rust remover for the iron deposits.
 
R

RGH269

Guest
I've been told the biggest difference between 20,30 or 40 is the speed at which they work I have also been told that adding amonia does the same to any of them. I have used them all straight and 50/50 or less amonia and couldn't tell much if any difference.
 

Derek

Supportive Member
Joined
Oct 7, 2006
Messages
2,166
Name
Derek
adding ammonia = something like stain magic.

if i remember right, i could easily be wrong.
 